Answer:
procedure attached below
The material to be used will have a %Cw of 34.5%Cw which is < 40%Cw
Step-by-step explanation:
Given data:
Minimum tensile strength = 865 MPa
Ductility = 10%EL
Desired Final diameter = 6.0 mm
20% cold worked 7.94 mm diameter 1040 steel stock
Describe the procedure you would follow to obtain this material.
assuming 1040 steel experiences cracking at 40%CW
attached below is a detailed procedure of obtaining the material
The material to be used will have a %Cw of 34.5%Cw which is < 40%Cw