Step-by-step explanation:
1.Plastic
Thermal Degradation – Plastic materials subjected to prolonged exposure to high temperatures will lose strength and toughness, becoming more prone to cracking, chipping, and breaking, at a rate in proportion to the temperature and time of exposure.
2.Iron
At room temperature, the iron atoms are in an unusual loosely packed open arrangement; as iron is heated past 912 degrees Celsius, the atoms become more closely packed before loosening again at 1,394 degrees Celsius and ultimately melting at 1,538 degrees Celsius