207,454 views
18 votes
18 votes
In the construction of a large reactor pressure vessel, a new steel alloy with a plane strain fracture toughness of 55 MPa-m1/2 and a Y value of 1.0. An in-service stress level of 200 MPa has been calculated. What is the length of a surface crack (in mm) that will lead to fracture

User Vinay Prabhakaran
by
2.9k points

1 Answer

8 votes
8 votes

Answer:


l=24mm

Step-by-step explanation:

From the question we are told that:

Plane strain fracture toughness of
T=55 MPa-m1/2

Y value
Y=1.0

Stress level of
\sigma =200 MPa

Generally the equation for length of a surface crack is mathematically given by


l=(1)/(\pi)((T)/(Y*\sigma))^2


l=(1)/(3.142)((55)/(1*200))^2


l=0.024m

Therefore

in mm


l=24mm

User JerseyMike
by
2.9k points